鋁卷在出貨前的質(zhì)量檢驗(yàn)有什么方法?

來源:http://www.igugo.cn/ 發(fā)布時(shí)間:2022-04-07

  
  鋁卷廠家生產(chǎn)鋁卷之后,要對(duì)成品進(jìn)行檢驗(yàn),這是板材生產(chǎn)出貨前的一道工序。那么鋁卷在出貨前的質(zhì)量檢驗(yàn)有什么方法?這個(gè)問題值得大家來了解了解。
  Aluminum coil manufacturers after the production of aluminum coil, to test the finished product, this is a process before the production and shipment of plate. So what is the method of quality inspection of aluminum coil before shipment? This is a question worth exploring.
  在經(jīng)過大量的加工過程后,不可避免地會(huì)產(chǎn)生各種缺陷和廢品。因此,按照相關(guān)標(biāo)準(zhǔn)來檢測(cè)板材的尺寸精度和表面質(zhì)量。超出標(biāo)準(zhǔn)規(guī)定的尺寸偏差對(duì)成品板材表面應(yīng)進(jìn)行光潔處理,邊緣不得有毛刺、裂紋、折角、磕碰等現(xiàn)象。表面缺陷須符合標(biāo)準(zhǔn)規(guī)定,須符合相關(guān)標(biāo)準(zhǔn)或技術(shù)條件的規(guī)定,并且光潔、無擦傷、劃傷等。
  After a large number of processing process, it will inevitably produce various defects and waste products. Therefore, in accordance with the relevant standards to detect the size of the sheet and surface quality. Beyond the standard size deviation of the finished plate surface should be smooth processing, the edge shall not have burr, crack, fold Angle, knock against and other phenomena. The surface defects shall meet the standards, the relevant standards or technical conditions, and be smooth, free from scratches, scratches, etc.
  平直度檢驗(yàn)鋼板表面質(zhì)量的方法是將受檢鋼板放置在檢驗(yàn)平臺(tái)上,用肉眼檢查鋼板表面是否有超出標(biāo)準(zhǔn)規(guī)定的缺陷,再檢查板材與平臺(tái)之間的間隙,不超過標(biāo)準(zhǔn)規(guī)定范圍的,即為合格成品。將合格的板材一端頭打上合號(hào)、狀態(tài)代號(hào)、厚度、批號(hào)、順序號(hào)和合格檢印等。
  The method of flatness inspection of surface quality of steel plate is to place the inspected steel plate on the inspection platform, check whether the surface of the steel plate has defects beyond the standard with the naked eye, and then check the gap between the plate and the platform. If it does not exceed the standard, it is qualified finished product. Alloy number, status code, thickness, batch number, serial number and qualified check mark shall be marked on one end of the qualified plate.


  鋁卷生產(chǎn)廠家認(rèn)為為檢驗(yàn)成品板的機(jī)械性能、內(nèi)部組織、工藝性能等,須按照標(biāo)準(zhǔn)和工藝規(guī)定的項(xiàng)目,對(duì)每一批次的產(chǎn)品進(jìn)行切割試驗(yàn),以保證板材的質(zhì)量符合產(chǎn)品標(biāo)準(zhǔn),滿足用戶的使用要求。
  Aluminum coil manufacturers think that in order to test the mechanical properties, internal organization, process performance of the finished plate, it is necessary to carry out cutting test on each batch of products in accordance with the standards and process requirements, so as to ensure that the quality of the plate meets the product standards and meet the requirements of users.
  對(duì)重要產(chǎn)品的機(jī)械性能進(jìn)行測(cè)試。如果在機(jī)械性能測(cè)試中發(fā)現(xiàn)一種樣品不合格,則對(duì)該不合格樣品的板材進(jìn)行二次重復(fù)試驗(yàn)。若再試樣中仍有一件不合格,則報(bào)廢。供方可逐張復(fù)驗(yàn)不合格樣品所代表的一段板材。交貨合格,不合格者視為無效。
  Test mechanical properties of important products. If a sample is found to be unqualified during the mechanical property test, a second repeat test is carried out on the plate of the unqualified sample. If there is still one unqualified sample, it will be scrapped. The supplier may retest one sheet at a time the section represented by the nonconforming sample. Unqualified delivery shall be deemed invalid.
  按照國家標(biāo)準(zhǔn)、行業(yè)標(biāo)準(zhǔn)、企業(yè)標(biāo)準(zhǔn)、技術(shù)條件、技術(shù)規(guī)程等規(guī)定,對(duì)產(chǎn)品的表面、機(jī)械性能等進(jìn)行全面檢查驗(yàn)收,確保向用戶提供優(yōu)質(zhì)鋁卷產(chǎn)品。更多內(nèi)容就來網(wǎng)站www.igugo.cn咨詢吧!
  In accordance with national standards, industrial standards, enterprise standards, technical conditions, technical regulations and other provisions, we carry out a comprehensive inspection and acceptance of the surface and mechanical properties of the products to ensure that we provide users with high-quality aluminum coil products. More content to the website www.igugo.cn consultation!